You are on page 1of 1

Messrs.

’: NATCON engineering and contracting Beirut 1/3/18


ATT: Mr. Roy Abou Diwan Ref: LT 1788 002 13 18
Project: Spears Lot 1788
Subject: repair of defective concrete at joint

Dear Sir,

In order to repair the defective concrete at joint location, krystol Plasti-Patch is to be used
according to the following:

- Wash the surface area to be repaired with clean water (remove any form release or
curing compounds).
Do not use an acid cleaner.
- Pour a 4 cm wide strip of krystol Plasti-Patch along the length of the defective joint
surface filling the voids in the concrete.
Note that a 6 mm thickness of Plasti- Patch is sufficient.

Best regards

Page 1 of 1