Florrea Gold Lixiviant GOLDIX 570--- Environmentally friendly Gold Leaching without cyanide.
Trade Name:
Synonyms: Gold leaching reagent , Lixiviant , Leachant , Florrea GOLDIX 570 ,Excellent 100% replacement for
sodium cyanide in gold leaching
Currently Florrea gold extraction reagent-- environmental protection has founded wide application in China. It
turns out to be reliable in performance. It is proved to be the same performance or even better than sodium
cyanide.
CASE STUDY 1
Comparison between Sodium cyanide and Goldix 570
Gold extracting
DosageAu 1.00.5g/t
pH
Chemical
Temperature
(gram/ton ore)
Sodium cyanide
Goldix 570
111
200~500
111
normal
200100
normal
CASE STUDY 2
Heap leaching result in a Chinese Heap filtering in a dry-pit
Gold Dissolving
Gold collecting
Time (Hour)
reagent
Tank:144h
Dump:1440h
tank:72h
heap:720h
exchange resin
Ore components
Au (g/ton)
Cu
As
Pb
TFe
Average assay
1.65
0.65
0.03
0.18
0.12
0.11
5.38
Heap
Gold
Ore
Concentration
Time of
Total
Average
Adsorption
Recovery
Leaching
Type
extracting
treated
of the reagent
spaying
amount
amount
rate
rate
rate
reagent
(ton)
()
(d)
of
Of
charcoal
Sodium
gold
gold
collected
extracted
(Gram)
(g/ton)
of
of
smeltering
12500
0.7
40
17780
1.42
97.8
98.3
89.58
12500
0.7
40
18700
1.50
98.2
98.4
93.83
cyanide
B
Goldix
570
CASE STUDY 3
Goldix 570 extracting reagent used in a Chinese Yunnan Gold Mine
Feeding gold assay: 1.28g/t
Particle size of heaped ore: -50mm;
Solid to liquid ratio: 2: 1
Dosage of quick lime: 1.5kg/t
Working concentration of Goldix 570: 0.7
Leaching time: 8 days
Leaching rate: 93.07%
Adsorption rate: 98.32%
Electro-analysis rate of resolution: 98%
Recovery rate of smeltering: 98%
Overall recovery rate: 87.88%
CASE STUDY 4
Goldix 570 extracting reagent used in a Chinese Yunnan Gold Mine
In September of 2010, Florrea Goldix 570 is used in the heap leaching production of oxidized gold ore of
one Chinese gold sites. It turns out to be reliable in performance and effective in use to replace sodium
cyanide completely.
Ore characteristics: Fine water permeability of oxidize mines, little impurities and easy leaching.
Ore volume of storage yard: 4000 mts
Average grade of gold ore: 0.5g/t
Period for Spraying: 40 days
Grade of tailings: 0.060.08g/t,
CASE STUDY 5
Goldix 570 extracting reagent used in a Chinese Gold Tailings
In October 2010, Goldix 570 is used for the gold tailings at four storage yards of the ore site.
Ore characteristics: large sediment percentage, poor permeability. After raking over the ore, Florrea Goldix 570 was used for leaching.
It is proved that Goldix 570 is compatible with sodium cyanide.
Ore storage of each story yard: 800012000 mts
Average tailing gold assay: around 0.23g/t
Period for spraying: 40 days
Tailing gold assay: 0.070.1g/t .
Leaching rate: 70 %.
CASE STUDY 6
Goldix 570 extracting reagent used in a Chinese Gold mine
As sodium cyanide is prohibited in this region in China, environmental protection has become a bottleneck for gold ore
manufacturing in the area. Oxidized ore of this gold deposit is faintly acid, and has
contains harmful elements such as like sulphur and arsenic, This ore is regarded as difficulty ore to process.
1
In May 2011,Plant trial using Florrea Goldix 570 environmental friendly gold extracting reagent is done in the Gold Mine.
The test ended in July 2011, lasting 50 days.
Gold Ore volume treated : 3000 mt.
Average gold assay at the storage yard: 0.48 g/t.
Spraying period: 40 days.
Tailing gold assay : 0.050.08g/t.
Leaching rate : 80 %
CASE STUDY 7
Goldix 570 extracting reagent used in a Chinese Gold mine
China YNMJ Gold Mine (large Gold Mine)
Annual gold ore processing volume : 1.5 million cubic meters.
Gold Mine production time with environmentally friendly Goldix 570: March 2012
Performance in leaching: It turned out to be reliable
CASE STUDY 8
Goldix 570 extracting reagent used in a Chinese Gold mine
GNDW Gold Mine (super huge gold mine)
In July 2011, large scale trial is conducted at the gold ore site involving more than 50,000 tons of ore with Florrea Goldix
570 environmental protection gold extraction reagent.
Ore volume at the storage yard: 50000 MT
Average GOLD feeding assay at the storage yard: 0.52 g/t
Spraying period: 40 days
Tailings grade: 0.030.08g/t.
Leaching rate: 80 %
CASE STUDY 10
Goldix 570 extracting reagent used in a Chinese GXLS
old mine
CASE STUDY 11
Goldix 570 extracting reagent used in a Chinese GXHK Gold mine ---HEAP LEACHING
Feeding oxide gold assay: 1.98g/t
Recovery rate: 89.83%
Gold extraction reagent: Florrea Goldix 570
Leaching method: large scale heap leaching
CASE STUDY 12
Goldix 570 extracting reagent used in a Chinese GZQD Gold mine ---LOW ASSAY HEAP SPAYING
Feeding oxide gold assay: 0.35g/t
Recovery rate: 85%
Gold extraction reagent: Florrea Goldix 570
Leaching method: large scale heap leaching