MANUFACTURER

LOW HYDROGEN ELECTRODES

HERMITICALLY PACKED

NON HERMITICALLY PACKED

BACKING OVEN MINIMUM 350 C @


2HRS MINIMUM

MARK WITH PERMANENT MARKER


AT STUB END

STORAGE OVEN MINIMUM


150 C @ CONTINUOUSLY

QUIVER MINIMUM 100C @


CONTINUOUSLY

R
E
B
A
K
E

ELECTRODES IN QUIVER
EXPOSURER TIME< 4 HRS

ELECTRODES CROSSED
4HRS TIME FROM ISSUE
REBAKED ELECTRODES
EXPOSURE > 8HRS

DISCARD